Euronorm EN EN X5CrNiMoTi17-12-2 Euronorm Stainless Steel and EN X5CrNiMoTi17-12-2 Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
Category | Type | Steel Grade | Standard | Country | Application |
---|---|---|---|---|---|
Steel Grades | Special Steel | EN X5CrNiMoTi17-12-2 | EN | Euronorm | Euronorm Stainless Steel |
EN X2CrNiMoCuWN25-7-4 |
|||||
EN X2CrNiMoN17-13-3 |
|||||
EN X2CrNiMoN17-13-5 |
|||||
EN X2CrNiMoN22-5-3 |
|||||
EN X2CrNiMoN25-7-4 |
|||||
EN X2CrNiNi8-10 |
|||||
EN X2CrNiN23-4 |
|||||
EN X3CrNiMo17-13-3 |
|||||
EN X5CrNi18-10 |
|||||
EN X5CrNiMo17-12-3 |
C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Ni(%) | Mo(%) | Ti(%) |
---|---|---|---|---|---|---|---|---|
0.08 | 1.00 | 2.00 | 0.045 | 0.015 | 16.5-18.5 | 10.5-13.5 | 2.00-2.50 | 5XC-0.70 |
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
145 (≥) | 224 (≥) | 21 | 21 | 23 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 114 |
Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
---|---|---|---|---|---|---|---|
12 | - | - | 0.32 | - | |||
731 | 815 | - | 24.3 | 443 | - | ||
148 | - | 34 | 43.2 | 414 | 232 |
Heat treated : 1944°C - 1478°C
Grade | Standard | Country | Application |
---|---|---|---|
EN X5CrNiMoTi17-12-2 | EN | Euronorm | Euronorm Stainless Steel |
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...
Rfq.: sales@longhaisteel.com