Euronorm EN EN X1NiCrMaCuN-25-20-7 Euronorm Stainless Steel and EN X1NiCrMaCuN-25-20-7 Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
Category | Type | Steel Grade | Standard | Country | Application |
---|---|---|---|---|---|
Steel Grades | Special Steel | EN X1NiCrMaCuN-25-20-7 | EN | Euronorm | Euronorm Stainless Steel |
EN X12CrNi2621KE |
|||||
EN X12CfNi3009KE |
|||||
EN X12CrNiSi2212KE |
|||||
EN X1SCrNiMn180SKE |
|||||
EN X1CrNi25-21 |
|||||
EN X1CrNiMoCuN-20-18-7 |
|||||
EN X1CrNiMoCuN-25-25-5 |
|||||
EN X1CrNiMoCuN-25-22-2 |
|||||
EN X1NiCrMoCu25-20-5 |
|||||
EN X1NiCrMoCu31-27-4 |
C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Ni(%) | Mo(%) | N(%) | Cu(%) |
---|---|---|---|---|---|---|---|---|---|
0.020 | 0.50 | 1.00 | 0.030 | 0.010 | 19.0-21.0 | 24.0-26.0 | 6.00-7.00 | 0.15-0.25 | 0.80-1.50 |
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
796 (≥) | 865 (≥) | 22 | 34 | 21 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 212 |
Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
---|---|---|---|---|---|---|---|
13 | - | - | 0.23 | - | |||
841 | 783 | - | 43.3 | 222 | - | ||
662 | - | 14 | 42.2 | 333 | 322 |
Heat treated : 1772°C - 1452°C
Grade | Standard | Country | Application |
---|---|---|---|
EN X1NiCrMaCuN-25-20-7 | EN | Euronorm | Euronorm Stainless Steel |
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...
Rfq.: sales@longhaisteel.com