Category | Type | Steel Grade | Standard | Country | Application |
---|---|---|---|---|---|
Steel Grades | Special Steel | 2304 | UNS | USA | Dual-phase steel |
3RE60 |
|||||
S31500 |
|||||
S31500 |
|||||
2205 |
|||||
2205 |
|||||
S31803 |
|||||
S31803 |
|||||
S32304 |
|||||
S32304 |
|||||
2304 |
C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Ni(%) | Mo(%) | N(%) | Cu(%) |
---|---|---|---|---|---|---|---|---|---|
0.03 | 1 | 2.5 | Max 0.04 | Max 0.04 | 21.5-24.5 | 3.0-5.5 | 0.05-0.60 | 0.05-0.20 | 0.05-0.60 |
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
333 (≥) | 698 (≥) | 31 | 41 | 41 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 112 |
Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
---|---|---|---|---|---|---|---|
23 | - | - | 0.23 | - | |||
598 | 898 | - | 33.3 | 334 | - | ||
284 | - | 34 | 33.2 | 111 | 232 |
Heat treated : 1498°C - 1787°C
Grade | Standard | Country | Application |
---|---|---|---|
S32304 | UNS | USA | Dual-phase steel |
S32304 | UNS | USA | Dual-phase steel |
2304 | UNS | USA | Dual-phase steel |
2304 | UNS | USA | Dual-phase steel |
SS 2304 | SS | Sweden | Swedish SS standard stainless steel and heat resistant steel |