Korea KS STS 202 KS standard austenite stainless steel bars(KS D3706-1992) and STS 202 Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
Category | Type | Steel Grade | Standard | Country | Application |
---|---|---|---|---|---|
Steel Grades | Special Alloy | STS 202 | KS | Korea | KS standard austenite stainless steel bars(KS D3706-1992) |
Ferrite 46 |
|||||
Martensite 1 |
|||||
Martensite 3 |
|||||
Martensite 4 |
|||||
Martensite 11 |
|||||
Martensite 600 |
|||||
Martensite 616 |
|||||
Austenitic 309 |
|||||
STS317LN |
|||||
STS201 |
C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Ni(%) | N(%) |
---|---|---|---|---|---|---|---|
Max 0.15 | Max 1.00 | 7.50-10.0 | Max 0.060 | Max 0.03 | 17.0-19.O | 4.00-6.OO | Max 0.25 |
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
612 (≥) | 471 (≥) | 42 | 24 | 42 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 432 |
Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
---|---|---|---|---|---|---|---|
22 | - | - | 0.14 | - | |||
358 | 884 | - | 31.3 | 432 | - | ||
579 | - | 13 | 14.2 | 232 | 142 |
Heat treated : 1491°C - 1112°C
Grade | Standard | Country | Application |
---|---|---|---|
STS 202 | KS | Korea | KS standard austenite stainless steel bars(KS D3706-1992) |
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...
Rfq.: sales@longhaisteel.com