ISO ISO ISO X7CrNiSiNCe21 11 ISO standard Austenite size heat resistant steel and ISO X7CrNiSiNCe21 11 Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
Category | Type | Steel Grade | Standard | Country | Application |
---|---|---|---|---|---|
Steel Grades | Special Alloy | ISO X7CrNiSiNCe21 11 | ISO | ISO | ISO standard Austenite size heat resistant steel |
ISO H6 |
|||||
ISO X15CrN26 |
|||||
ISO H7 |
|||||
ISO X7CrNi18 9 |
|||||
ISO H10 |
|||||
ISO X7CrNiTi18 10 |
|||||
ISO H11 |
|||||
ISO X7CrNiNb18 10 |
|||||
ISO H12 |
|||||
ISO X15CrNiSi20 12 |
C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Ni(%) | N(%) | Other(%) |
---|---|---|---|---|---|---|---|---|
Max 0.10 | 1.4-2.0 | Max 0.8 | Max 0.045 | Max 0.030 | 20.0-22.0 | 10.0-12.0 | 0.14-0.20 | Ce:0.03-0.08 |
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
444 (≥) | 971 (≥) | 23 | 32 | 43 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 124 |
Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
---|---|---|---|---|---|---|---|
34 | - | - | 0.41 | - | |||
426 | 715 | - | 22.3 | 244 | - | ||
566 | - | 24 | 12.2 | 444 | 113 |
Heat treated : 1354°C - 1892°C
Grade | Standard | Country | Application |
---|---|---|---|
ISO X7CrNiSiNCe21 11 | ISO | ISO | ISO standard Austenite size heat resistant steel |
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...
Rfq.: sales@longhaisteel.com