China GBT GH4413 wrought Fe/Ni-base superalloy and GH4413 Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
Category | Type | Steel Grade | Standard | Country | Application |
---|---|---|---|---|---|
Steel Grades | Special Alloy | GH4413 | GBT | China | wrought Fe/Ni-base superalloy |
GH4105 |
|||||
GH4133 |
|||||
GH4133B |
|||||
GH4141 |
|||||
GH4145 |
|||||
GH4163 |
|||||
GH4169 |
|||||
GH4199 |
|||||
GH4202 |
|||||
GH4220 |
C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Ni(%) | Mo(%) | W(%) | Cu(%) | B(%) | Al(%) | Ti(%) | La(%) | Fe(%) |
---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
0.04-0. 10 | 0. 60 | 0.50 | 0+015 | 0.009 | 13.00-16.00 | Bal | 2.50-4.00 | 5.00-7.00 | 0.070 | 0.020 | 2.40 - 2.90 | 1.70 -2.20 | 0.200 -1.000 | ≤5.00 |
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
397 (≥) | 471 (≥) | 41 | 12 | 32 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 442 |
Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
---|---|---|---|---|---|---|---|
41 | - | - | 0.42 | - | |||
498 | 563 | - | 24.3 | 232 | - | ||
142 | - | 11 | 31.2 | 424 | 343 |
Heat treated : 1298°C - 1193°C