China GBT GH4202 wrought Fe/Ni-base superalloy and GH4202 Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
Category | Type | Steel Grade | Standard | Country | Application |
---|---|---|---|---|---|
Steel Grades | Special Alloy | GH4202 | GBT | China | wrought Fe/Ni-base superalloy |
GH4098 |
|||||
GH4099 |
|||||
GH4105 |
|||||
GH4133 |
|||||
GH4133B |
|||||
GH4141 |
|||||
GH4145 |
|||||
GH4163 |
|||||
GH4169 |
|||||
GH4199 |
C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Ni(%) | Mo(%) | V(%) | W(%) | Cu(%) | Co(%) | B(%) | Nb(%) | Al(%) | Ti(%) | Fe(%) |
---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
≤0.08 | 0. 60 | 0.50 | 0.015 | 0.010 | 17.00-20.00 | Bal | 4.00-5.00 | - | 4.00-5.00 | - | - | ≤0.010 | - | 1.00-1. 50 | 2. 20-2.80 | ≤4.00 |
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
672 (≥) | 979 (≥) | 23 | 12 | 21 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 434 |
Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
---|---|---|---|---|---|---|---|
33 | - | - | 0.41 | - | |||
234 | 381 | - | 31.3 | 214 | - | ||
828 | - | 13 | 23.2 | 123 | 433 |
Heat treated : 1897°C - 1397°C
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...