Korea KS STS329J1 Austenitic Steel and STS329J1 Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
| Category | Type | Steel Grade | Standard | Country | Application |
|---|---|---|---|---|---|
| Steel Grades | Heat-Resistant Steel | STS329J1 | KS | Korea | Austenitic Steel |
| 31X19H9MBБT |
|||||
| 36X18H25C2 |
|||||
| 55X20Γ9AH4 |
|||||
| 07X12Γ7AH5 |
|||||
| 03X21H21M4Γ |
|||||
| 45X22H4M3 |
|||||
| 10X23H18 |
|||||
| 20X23H18 |
|||||
| 20X25H20C2 |
|||||
| l2X25H16Γ7AP |
| C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Ni(%) | Mo(%) |
|---|---|---|---|---|---|---|---|
| Max 0.08 | Max 1.00 | Max 1.50 | Max 0.04 | Max O.030 | 23.0-28.0 | 3.OO-6.00 | 1.00-3.00 |
| Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
|---|---|---|---|---|---|---|
| 844 (≥) | 265 (≥) | 14 | 31 | 12 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 441 |
| Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
|---|---|---|---|---|---|---|---|
| 13 | - | - | 0.22 | - | |||
| 368 | 159 | - | 13.3 | 143 | - | ||
| 322 | - | 11 | 23.2 | 143 | 323 |
Heat treated : 1112°C - 1824°C
| Grade | Standard | Country | Application |
|---|---|---|---|
| STS329J1 | KS | Korea | Austenitic Steel |
| STS329J1 | KS | Korea | Austenitic Steel |