Russia ГОСТ 36X18H25C2 Austenitic and 36X18H25C2 Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
Category | Type | Steel Grade | Standard | Country | Application |
---|---|---|---|---|---|
Steel Grades | Heat-Resistant Steel | 36X18H25C2 | ГОСТ | Russia | Austenitic |
08X18H10T |
|||||
12X18H10T |
|||||
12X18H10E |
|||||
03X18H11 |
|||||
06X18H11 |
|||||
03X18H12 |
|||||
03X18H12T |
|||||
12X18H12T |
|||||
08X18H12Б |
|||||
31X19H9MBБT |
C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Ni(%) | Mo(%) | W(%) | Ti(%) |
---|---|---|---|---|---|---|---|---|---|
0.32-0.40 | 2.00-3.00 | Max 1.50 | Max 0.035 | Max 0.02 | 17.0-19.0 | 23.0-26.0 | Max 0.30 | Max 0.20 | Max 0.20 |
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
874 (≥) | 253 (≥) | 23 | 22 | 24 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 123 |
Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
---|---|---|---|---|---|---|---|
23 | - | - | 0.42 | - | |||
233 | 837 | - | 44.3 | 433 | - | ||
139 | - | 33 | 32.2 | 244 | 434 |
Heat treated : 1324°C - 1256°C
Grade | Standard | Country | Application |
---|---|---|---|
36X18H25C2 | ГОСТ | Russia | Austenitic |
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...