Commonly used materials approximate limit strength

materials Fatigue and compressive limit Bending fatigue limit Reverse fatigue limit Pull pressure pulsation fatigue limit Bending pulse fatigue limit Reverse pulse fatigue limit
Structural steel ≈0.3σb ≈0.43σb ≈0.25σb ≈1.42σ-11 ≈1.33σ-1 ≈1.5τ-1
Cast iron ≈0.225σb ≈0.45σb ≈0.36σb ≈1.42σ-11 ≈1.35σ-1 ≈1.35τ-1
Aluminum alloy ≈σb/6+73.5MPa ≈σb/6+73.5MPa ≈(0.55~0.58)σ-1 ≈1.5σ-11    
Structural steel ≈0.3σb ≈0.43σb ≈0.25σb ≈1.42σ-11 ≈1.33σ-1 ≈1.5τ-1
Cast iron ≈0.225σb ≈0.45σb ≈0.36σb ≈1.42σ-11 ≈1.35σ-1 ≈1.35τ-1
Aluminum alloy ≈σb/6+73.5MPa ≈σb/6+73.5MPa ≈(0.55~0.58)σ-1 ≈1.5σ-11    