Germany DIN X10CrNiMoNb18-12 Stainless steel and X10CrNiMoNb18-12 Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
| Category | Type | Steel Grade | Standard | Country | Application |
|---|---|---|---|---|---|
| Steel Grades | Special Steel | X10CrNiMoNb18-12 | DIN | Germany | Stainless steel |
| W-Nr 1.4573 |
|||||
| X1CrNiMoNb28-4-2 |
|||||
| W-Nr 1.4575 |
|||||
| X3CrNiMoTi25-25 |
|||||
| W-Nr 1.4577 |
|||||
| W-Nr 1.4580 |
|||||
| X6CrNiMoNb17-12-2 |
|||||
| W-Nr 1.4582 |
|||||
| X4CrNiMoN25-7 |
|||||
| W-Nr 1.4583 |
| C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Ni(%) | Mo(%) | Nb(%) |
|---|---|---|---|---|---|---|---|---|
| Max 0.10 | Max 1.00 | Max 2.00 | Max 0.045 | Max 0.030 | 12.0-14.5 | 12.0-14.5 | 2.50-3.00 | Mix 8×C%① |
| Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
|---|---|---|---|---|---|---|
| 327 (≥) | 322 (≥) | 12 | 13 | 21 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 323 |
| Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
|---|---|---|---|---|---|---|---|
| 11 | - | - | 0.31 | - | |||
| 765 | 536 | - | 44.3 | 442 | - | ||
| 489 | - | 44 | 34.2 | 314 | 234 |
Heat treated : 1265°C - 1435°C
| Grade | Standard | Country | Application |
|---|---|---|---|
| X10CrNiMoNb18-12 | DIN | Germany | Stainless steel |
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...