Japan DIN SUS3386LTP austenitic special steel and SUS3386LTP Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
| Category | Type | Steel Grade | Standard | Country | Application |
|---|---|---|---|---|---|
| Steel Grades | Special Steel | SUS3386LTP | DIN | Japan | austenitic special steel |
| SUS309TP |
|||||
| SUS309STP |
|||||
| SUS310TP |
|||||
| SUS310STP |
|||||
| SUS316TP |
|||||
| SUS316HTP |
|||||
| SUS316LTP |
|||||
| SUS316TiTP |
|||||
| SUS317TP |
|||||
| SUS317LTP |
| C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Ni(%) | Mo(%) | N(%) |
|---|---|---|---|---|---|---|---|---|
| Max 0.03 | Max 1.00 | Max 2.00 | Max 0.04 | Max 0.03 | 19.00-24.00 | 24.00-26.00 | 5.00-7.00 | Max 0.25 |
| Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
|---|---|---|---|---|---|---|
| 823 (≥) | 761 (≥) | 14 | 44 | 32 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 214 |
| Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
|---|---|---|---|---|---|---|---|
| 44 | - | - | 0.31 | - | |||
| 832 | 435 | - | 32.3 | 341 | - | ||
| 716 | - | 42 | 41.2 | 123 | 434 |
Heat treated : 1119°C - 1363°C
| Grade | Standard | Country | Application |
|---|---|---|---|
| SUS3386LTP | DIN | Japan | austenitic special steel |
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...