USA ASTM H10 Tool Die Steels Hot-Work Tool Steel and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
Category | Class | Grade | Standard | Country | Application |
---|---|---|---|---|---|
Steel Grades | Tool Die Steels | H10 | ASTM | USA | Hot-Work Tool Steel |
C | Si | Mn | P | S | Cr | Mo | V | W | Ni+Cu |
---|---|---|---|---|---|---|---|---|---|
0.35 -0.45 | 0.80 -1.20 | 0.25 -0.70 | ≤0.030 | ≤0.030 | 3.00 -3.75 | 2.00 -3.00 | 0.25 -0.75 | ≤ ≥ | ≤0.75 |
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
957 (≥) | 758 (≥) | 33 | 22 | 32 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 114 |
Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
---|---|---|---|---|---|---|---|
21 | - | - | 0.23 | - | |||
835 | 963 | - | 21.3 | 221 | - | ||
861 | - | 32 | 42.2 | 441 | 411 |
Heat treated : 1927°C - 1627°C
Grade | Standard | Country | Application |
---|---|---|---|
UNS H10380 | |||
UNS H10450 | |||
UNS H10380 | |||
UNS H10450 | |||
ASTM H10 | |||
ASTM CH10 | |||
ASTM CPH10 | |||
AWS EH10K | |||
SWRCH10R | |||
SWRCH10A | |||
SWRCH10K | |||
SKH10 | |||
SKH10 | |||
:BH10 | |||
:BH10 | |||
BH10A | |||
BH10A | |||
04X18H10 | |||
08X18H10 | |||
08X18H10T |
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...
Rfq.: sales@longhaisteel.com