China GB GH4302 Superalloys Nickel-base superalloy and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.

Datasheet for: Steel Grades:Superalloys: GH4302
Category Class Grade Standard Country Application
Steel GradesSuperalloys GH4302 GB China Nickel-base superalloy

Chemical composition(mass fraction)(wt.%) of the GH4302

C Cr Mo Ni W Al Ti B Mn Ce Zr
≤0.08 12.0 -16.0 1.5 -2.5 38.0 -42.0 3.5 -4.5 1.8 -2.3 2.3 -2.8 ≤0.01 ≤0.6 ≤0.02 ≤0.05

Mechanical Properties of steel grade GH4302

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV/Ku (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
294 (≥) 451 (≥) 43 32 22 Solution and Aging, Annealing, Ausaging, Q+T,etc 431

Physical Properties of steel grade GH4302

Temperature
(°C)
Modulus of elasticity
(GPa)
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and Thermal conductivity
(W/m·°C)
Specific thermal capacity
(J/kg·°C)
Specific electrical resistivity
(Ω mm²/m)
Density
(kg/dm³)
Poisson’s coefficient, ν
33 - -     0.11 -  
318 471 - 12.3 444   -  
986 - 23 14.2   314 423

Heat Treatment of steel grade GH4302

Heat treated : 1166°C - 1812°C

Technological Curves of steel grade GH4302

Cross Reference Table (Equivalent Grade) of GH4302

Grade Standard Country Application
GH4302
GH4302

Available Suppliers

Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...

Rfq.: sales@longhaisteel.com
  • Do you supply this GH4302?
  • List your company on S&G now? Join
  • Non-paying users only
Top