Description

China GB GH4220 Superalloys Nickel-base superalloy and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.

Datasheet for: Steel Grades:Superalloys: GH4220
Category Class Grade Standard Country Application
Steel GradesSuperalloys GH4220 GB China Nickel-base superalloy

Chemical composition(mass fraction)(wt.%) of the GH4220

C Cr Mo Ni Co W Al Ti B Fe V Mg
≤0.08 9.0 -12.0 5.0 -7.0 ≤Remainder 14.0 -15.0 5.0 -6.5 3.9 -4.8 2.2 -2.9 ≤0.02 ≤3.0 0.2 -0.8 ≤trace

Mechanical Properties of steel grade GH4220

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV/Ku (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
525 (≥) 516 (≥) 42 13 44 Solution and Aging, Annealing, Ausaging, Q+T,etc 212

Physical Properties of steel grade GH4220

Temperature
(°C)
Modulus of elasticity
(GPa)
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and Thermal conductivity
(W/m·°C)
Specific thermal capacity
(J/kg·°C)
Specific electrical resistivity
(Ω mm²/m)
Density
(kg/dm³)
Poisson’s coefficient, ν
34 - -     0.14 -  
754 696 - 42.3 142   -  
983 - 41 14.2   313 112

Heat Treatment of steel grade GH4220

Heat treated : 1294°C - 1338°C

Technological Curves of steel grade GH4220

Cross Reference Table (Equivalent Grade) of GH4220

Grade Standard Country Application
GH4220
GH4220

Available Suppliers

Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...