Korea KS D 3758 (2003), NCF625TP Specialsteel Seamless nickel-chromium-iron alloy pipes and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
Category | Class | Grade | Standard | Country | Application |
---|---|---|---|---|---|
Steel Grades | Specialsteel | NCF625TP | KS | Korea | Seamless nickel-chromium-iron alloy pipes |
C | Si | Mn | P | S | Cr | Ni | Cu | Al | Ti | Fe | Nb+Ta | Mo |
---|---|---|---|---|---|---|---|---|---|---|---|---|
≤0.10 | ≤0.50 | ≤0.50 | ≤0.015 | ≤0.015 | 20.00 -23.00 | 58.00 - ≥ | ≤ ≥ | ≤0.40 | ≤0.40 | ≤5.00 | 3.15 -4.15 | 8.00 -10.00 |
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
532 (≥) | 572 (≥) | 43 | 21 | 44 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 113 |
Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
---|---|---|---|---|---|---|---|
41 | - | - | 0.33 | - | |||
747 | 865 | - | 13.3 | 243 | - | ||
127 | - | 33 | 22.2 | 331 | 211 |
Heat treated : 1449°C - 1241°C
Grade | Standard | Country | Application |
---|---|---|---|
NCF625 | |||
NCF625 TP | |||
NCF625 TB | |||
NCF625 TB | |||
NCF625 TP | |||
NCF625 | |||
NCF625 | |||
NCF625 | |||
NCF625TB | |||
NCF625TB | |||
NCF625TP | |||
NCF625TP |
D 3758 (2003) | Seamless nickel-chromium-iron alloy pipes | D-3758-(2003).pdf |
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...
Rfq.: sales@longhaisteel.com