NCF625 Stainless Steel and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
| Category | Type | Steel Grade | Standard | Country | Application | 
|---|---|---|---|---|---|
| Steel Grades | Stainless Steel | NCF625 | |||
| SUH661 | |||||
| SUH446 | |||||
| SUH1 | |||||
| SUH3 | |||||
| SUH4 | |||||
| SUH11 | |||||
| SUH600 | |||||
| SUH616 | |||||
| NCF600 | |||||
| NCF601 | 
| C ≤ | Si ≤ | Mn ≤ | P ≤ | S ≤ | Cr | Ni | 
|---|---|---|---|---|---|---|
| 0.1 | 0.5 | 0.5 | 0.015 | 0.015 | 20-23 | ≥58 | 
| Mo | Al | Cu | Nb+Ta | Ti | V | Ce | 
| 8-10 | ≤0.4 | 3.15-4.15 | ≤ 0.4 | ≤5.0 | ||
| N | Co | Pb | B | Other | ||
| Yield Rp0.2 (MPa) | Tensile Rm (MPa) | Impact KV/Ku (J) | Elongation A (%) | Reduction in cross section on fracture Z (%) | As-Heat-Treated Condition | Brinell hardness (HBW) | 
|---|---|---|---|---|---|---|
| 587 (≥) | 523 (≥) | 23 | 42 | 11 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 143 | 
| Temperature (°C) | Modulus of elasticity (GPa) | Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) | Specific thermal capacity (J/kg·°C) | Specific electrical resistivity (Ω mm²/m) | Density (kg/dm³) | Poisson’s coefficient, ν | 
|---|---|---|---|---|---|---|---|
| 31 | - | - | 0.42 | - | |||
| 428 | 285 | - | 14.3 | 312 | - | ||
| 944 | - | 13 | 41.2 | 331 | 132 | 
Heat treated : 1728°C - 1957°C
| Grade | Standard | Country | Application | 
|---|---|---|---|
| NCF625 | JIS | Japan | ferritic stainless steel | 
| NCF625TB | JIS | Japan | ferritic stainless steel | 
| NCF625TP | JIS | Japan | ferritic stainless steel | 