USA SAE A 813/A 813M (2009) , A 813 Grade TP 304L Specialsteel Single- or Double-Welded Austenitic Stainless Steel Pipe and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
Category | Class | Grade | Type | Standard | Country | Application |
---|---|---|---|---|---|---|
Steel Grades | Specialsteel | A 813 Grade TP 304L | Austenite | SAE | USA | Single- or Double-Welded Austenitic Stainless Steel Pipe |
C | Si | Mn | P | S | Cr | Ni |
---|---|---|---|---|---|---|
≤0.030 | ≤1.00 | ≤2.00 | ≤0.045 | ≤0.03 | 17.50 -19.50 | 8.00 -12.0 |
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
744 (≥) | 433 (≥) | 11 | 41 | 14 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 344 |
Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
---|---|---|---|---|---|---|---|
14 | - | - | 0.44 | - | |||
874 | 575 | - | 21.3 | 124 | - | ||
727 | - | 32 | 34.2 | 233 | 142 |
Heat treated : 1973°C - 1966°C
Grade | Standard | Country | Application |
---|---|---|---|
304L | |||
304LN | |||
304LHN | |||
AL 304L | |||
304L | |||
304LN | |||
TP304L | |||
TP304LN | |||
TP304L | |||
TP304LN | |||
TP304L | |||
TP304LN | |||
TP304L | |||
TP304LN | |||
TP304L | |||
MT304L | |||
MT-304L | |||
TP304L | |||
TP304LN | |||
304L |
A 813/A 813M (2009) | Single- or Double-Welded Austenitic Stainless Steel Pipe | A-813-A-813M--(2009)-.pdf |
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...
Rfq.: sales@longhaisteel.com