USA UNS SAE AMS 5342E (2006) , SAE AMS 5343E (2006) , SAE AMS 5344F (2007) , SAE AMS 5604G (2013) , SAE AMS 5622F (2013) , SAE AMS 5643/H1150 (2013) , SAE AMS 5643S (2013) , SAE J 467 (1968) , 17-4PH Specialsteel Steel, Corrosion-Resistant, Investment Castings 16Cr - 4.1Ni - 0.28Cb (Nb) - 3.2Cu Homogenization, Solution, and Precipitation Heat Treated (H1100) 130 ksi (896 MPa) Tensile Strength (17-4) and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
Category | Class | Grade | Type | Standard | Country | Application |
---|---|---|---|---|---|---|
Steel Grades | Specialsteel | 17-4PH | Precipitation-Hardening | UNS | USA | Steel, Corrosion-Resistant, Investment Castings 16Cr - 4.1Ni - 0.28Cb (Nb) - 3.2Cu Homogenization, Solution, and Precipitation Heat Treated (H1100) 130 ksi (896 MPa) Tensile Strength (17-4) |
C | Si | Mn | Cr | Ni | Cu | Nb |
---|---|---|---|---|---|---|
≤0.07 | ≤1.00 | ≤1.00 | 15.00 -17.50 | 3.00 -5.00 | 3.00 -5.00 | 0.15 -1.45 |
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
646 (≥) | 353 (≥) | 33 | 21 | 31 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 113 |
Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
---|---|---|---|---|---|---|---|
23 | - | - | 0.23 | - | |||
761 | 875 | - | 12.3 | 221 | - | ||
444 | - | 41 | 42.2 | 113 | 224 |
Heat treated : 1282°C - 1242°C
Grade | Standard | Country | Application |
---|---|---|---|
17-4PH | |||
17-4PH | |||
17-4PH(630) Steel for Turbine Blades |
SAE AMS 5342E (2006) | Steel, Corrosion-Resistant, Investment Castings 16Cr - 4.1Ni - 0.28Cb (Nb) - 3.2Cu Homogenization, Solution, and Precipitation Heat Treated (H1100) 130 ksi (896 MPa) Tensile Strength (17-4) | SAE-AMS-5342E-(2006)-.pdf |
SAE AMS 5343E (2006) | Steel, Corrosion-Resistant, Investment Castings 16Cr - 4.1Ni - 0.28Cb (Nb) - 3.2Cu Homogenization, Solution, and Precipitation Heat Treated (H1000) 150 ksi (1034 MPa) Tensile Strength (17-4) | SAE-AMS-5343E-(2006)-.pdf |
SAE AMS 5344F (2007) | Steel, Corrosion-Resistant, Investment Castings 16Cr - 4.1Ni - 0.28Cb - 3.2Cu Homogenization, Solution, and Precipitation Heat Treated (H900) 180 ksi (1241 MPa) Tensile Strength (17-4) | SAE-AMS-5344F-(2007)-.pdf |
SAE AMS 5604G (2013) | Steel, Corrosion Resistant, Sheet, Strip, and Plate 16.5Cr - 4.0Ni - 4.0Cu - 0.30Cb Solution Heat Treated, Precipitation Hardenable | SAE-AMS-5604G-(2013)-.pdf |
SAE AMS 5622F (2013) | Steel, Corrosion-Resistant, Bars, Wire, Forgings, Tubing, and Rings 16Cr - 4.0Ni - 0.30Cb - 4.0Cu Solution Heat Treated, Precipitation Hardenable Consumable Electrode Remelted | SAE-AMS-5622F-(2013)-.pdf |
SAE AMS 5643/H1150 (2013) | Steel, Corrosion-Resistant, Bars, Wire, Forgings, Tubing and Rings 16Cr – 4.0Ni – 0.30Cb (Nb) – 4.0Cu Solution and Precipitation Heat Treated (H1150) | SAE-AMS-5643-H1150-(2013)-.pdf |
SAE AMS 5643S (2013) | Steel, Corrosion-Resistant, Bars, Wire, Forgings, Tubing, and Rings 16Cr - 4.0Ni - 0.30Cb - 4.0Cu Solution Heat Treated, Precipitation Hardenable | SAE-AMS-5643S-(2013)-.pdf |