USA SAE A 814/A 814M (2008), A 814 S24000 Specialsteel Cold-Worked Welded Austenitic Stainless Steel Pipe and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
Category | Class | Grade | Type | Standard | Country | Application |
---|---|---|---|---|---|---|
Steel Grades | Specialsteel | A 814 S24000 | Austenite | SAE | USA | Cold-Worked Welded Austenitic Stainless Steel Pipe |
C | Mn | Si | P | S | Cr | Ni | Mo | N |
---|---|---|---|---|---|---|---|---|
≤0.08 | 11.50 -14.50 | ≤1.00 | ≤0.06 | ≤0.03 | 17.00 -19.00 | 2.50 -3.75 | ≤ ≥ | 0.20 -0.40 |
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
855 (≥) | 762 (≥) | 41 | 44 | 12 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 333 |
Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
---|---|---|---|---|---|---|---|
21 | - | - | 0.31 | - | |||
327 | 248 | - | 14.3 | 222 | - | ||
283 | - | 42 | 42.2 | 331 | 121 |
Heat treated : 1347°C - 1721°C
Grade | Standard | Country | Application |
---|---|---|---|
NITRONIC 20 | |||
NITRONIC 30 | |||
NITRONIC 32 | |||
NITRONIC 33 | |||
NITRONIC 40 | |||
NITRONIC 50 | |||
NITRONIC 60 | |||
S24000 | |||
S24000 | |||
S24000 | |||
S24000 | |||
S24000 | |||
S24000 | |||
S24000 |
A 814/A 814M (2008) | Cold-Worked Welded Austenitic Stainless Steel Pipe | A-814-A-814M-(2008).pdf |
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...
Rfq.: sales@longhaisteel.com