HS6-5-2S Tool Steel and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
| Category | Type | Steel Grade | Standard | Country | Application |
|---|---|---|---|---|---|
| Steel Grades | Tool Steel | HS6-5-2S | |||
| S 12-1-2 |
|||||
| 1.3318 |
|||||
| 1.3333 |
|||||
| S 3-3-2 |
|||||
| HS3-3-2 |
|||||
| 1.3340 |
|||||
| SC 6-5-2S |
|||||
| HS6-5-2CS |
|||||
| S 6-5-2 S |
|||||
| 1.3341 |
| C |
Si ≤ |
Mn ≤ |
P ≤ |
S ≤ |
Cr | Ni | Mo | Other |
|---|---|---|---|---|---|---|---|---|
| 0.86-0.94 | 0.45 | 0.40 | 0.030 | 0.06-0.15 | 3.80-4.50 | 4.70-5.20 |
W 6.00-6.70 V 1.70-2.00 Co 4.50-5.00 |
| Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
|---|---|---|---|---|---|---|
| 155 (≥) | 287 (≥) | 41 | 34 | 43 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 112 |
| Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
|---|---|---|---|---|---|---|---|
| 14 | - | - | 0.33 | - | |||
| 218 | 212 | - | 12.3 | 331 | - | ||
| 862 | - | 12 | 21.2 | 223 | 142 |
Heat treated : 1125°C - 1189°C