Germany DIN X220CrVMo12-2 Cold working alloy tool steel and X220CrVMo12-2 Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
Category | Type | Steel Grade | Standard | Country | Application |
---|---|---|---|---|---|
Steel Grades | Tool Steel And Hard Alloy | X220CrVMo12-2 | DIN | Germany | Cold working alloy tool steel |
1.2361 |
|||||
X91CrMoV18 |
|||||
1.2362 |
|||||
X63CrMoV5-1 |
|||||
X100CrMoV5-1 |
|||||
1.2363 |
|||||
1.2369 |
|||||
81MoCrV42-16 |
|||||
X96CrMoV12 |
|||||
1.2376 |
C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Mo(%) | V(%) |
---|---|---|---|---|---|---|---|
2.15-2.30 | 0.15-0.30 | 0.25-0.40 | Max 0.035 | Max 0.035 | 12.0-13.0 | 0.80-1.00 | 2.00-2.30 |
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
249 (≥) | 714 (≥) | 13 | 41 | 32 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 313 |
Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
---|---|---|---|---|---|---|---|
23 | - | - | 0.11 | - | |||
233 | 185 | - | 32.3 | 331 | - | ||
937 | - | 43 | 43.2 | 324 | 123 |
Heat treated : 1621°C - 1226°C
Grade | Standard | Country | Application |
---|---|---|---|
X220CrVMo12-2 | DIN | Germany | Cold working alloy tool steel |