Germany DIN X20CrMo13 Hot working alloy tool steel and X20CrMo13 Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
| Category | Type | Steel Grade | Standard | Country | Application |
|---|---|---|---|---|---|
| Steel Grades | Tool Steel And Hard Alloy | X20CrMo13 | DIN | Germany | Hot working alloy tool steel |
| X23CrNi17 |
|||||
| 1.2787 |
|||||
| X32CrMoCoV3-3-3 |
|||||
| 1.2885 |
|||||
| X15CrMoCoV10-10-5 |
|||||
| 1.2886 |
|||||
| X20CoCrWMo10-9 |
|||||
| 1.2888 |
|||||
| X45CoCrMoV5-5-3 |
|||||
| 1.2889 |
| C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Ni(%) | Mo(%) |
|---|---|---|---|---|---|---|---|
| 0.17-0.22 | Max 1.00 | Max 1.00 | Max 0.045 | Max 0.030 | 12.0-14.0 | Max 1.00 | 0.90-1.30 |
| Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
|---|---|---|---|---|---|---|
| 566 (≥) | 923 (≥) | 31 | 24 | 22 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 214 |
| Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
|---|---|---|---|---|---|---|---|
| 23 | - | - | 0.41 | - | |||
| 568 | 943 | - | 43.3 | 131 | - | ||
| 311 | - | 22 | 22.2 | 224 | 144 |
Heat treated : 1927°C - 1549°C