China W6Mo5Cr4V3 High-speed tool steel and W6Mo5Cr4V3 Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
| Category | Type | Steel Grade | Standard | Country | Application |
|---|---|---|---|---|---|
| Steel Grades | Tool Steel And Hard Alloy | W6Mo5Cr4V3 | China | High-speed tool steel | |
| SM3Cr17Mo |
|||||
| SM4Cr13 |
|||||
| SM45A |
|||||
| SM48 |
|||||
| W18Cr4V |
|||||
| W18Cr4VCo8 |
|||||
| W18Cr4V2Co8 |
|||||
| W12Cr4V5Co5 |
|||||
| W6Mo5Cr4V2 |
|||||
| CW6Mo5Cr4V2 |
| C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Mo(%) | V(%) | W(%) |
|---|---|---|---|---|---|---|---|---|
| 1.00~1.10 | 0.20~0.45 | 0.15~0.40 | ≤0.030 | ≤0.030 | 3.75~4.50 | 4.75~6.50 | 2.25~2.75 | 5.00~6.75 |
| Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
|---|---|---|---|---|---|---|
| 672 (≥) | 263 (≥) | 23 | 21 | 44 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 334 |
| Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
|---|---|---|---|---|---|---|---|
| 22 | - | - | 0.33 | - | |||
| 373 | 426 | - | 31.3 | 313 | - | ||
| 587 | - | 31 | 31.2 | 233 | 112 |
Heat treated : 1399°C - 1247°C
| Grade | Standard | Country | Application |
|---|---|---|---|
| W6Mo5Cr4V3 | China | High-speed tool steel | |
| CW6Mo5Cr4V3 | China | High-speed tool steel |