USA UNS T11352 The middle of high-speed tool steel and T11352 Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
Category | Type | Steel Grade | Standard | Country | Application |
---|---|---|---|---|---|
Steel Grades | Tool Steel And Hard Alloy | T11352 | UNS | USA | The middle of high-speed tool steel |
T11344 |
|||||
M46 |
|||||
T11346 |
|||||
M47 |
|||||
T11347 |
|||||
M48 |
|||||
M62 |
|||||
M50 |
|||||
T11350 |
|||||
M52 |
C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Mo(%) | V(%) | W(%) |
---|---|---|---|---|---|---|---|---|
0.85~0.95 | 0.20~0.60 | 0.15~0.45 | MAX 0.030 | MAX 0.030 | 3.50~4.30 | 4.00~4.90 | 1.65~2.25 | 0.75~1.50 |
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
588 (≥) | 857 (≥) | 41 | 42 | 43 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 411 |
Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
---|---|---|---|---|---|---|---|
42 | - | - | 0.33 | - | |||
117 | 936 | - | 21.3 | 244 | - | ||
624 | - | 11 | 13.2 | 123 | 124 |
Heat treated : 1689°C - 1165°C
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...