Japan JIS K30 Carbide for cutting tools and K30 Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
Category | Type | Steel Grade | Standard | Country | Application |
---|---|---|---|---|---|
Steel Grades | Tool Steel And Hard Alloy | K30 | JIS | Japan | Carbide for cutting tools |
P30 |
|||||
P40 |
|||||
BW1A |
|||||
M10 |
|||||
M20 |
|||||
M30 |
|||||
M40 |
|||||
K01 |
|||||
K10 |
|||||
K20 |
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
766 (≥) | 962 (≥) | 32 | 33 | 31 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 141 |
Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
---|---|---|---|---|---|---|---|
43 | - | - | 0.34 | - | |||
826 | 436 | - | 44.3 | 234 | - | ||
955 | - | 32 | 21.2 | 344 | 324 |
Heat treated : 1793°C - 1142°C
Grade | Standard | Country | Application |
---|---|---|---|
K30 | JIS | Japan | Carbide for cutting tools |
ASTM HK30 | AISI | USA | |
HK30 | ASTM | USA | Steel Castings, Iron-Chromium and Iron-Chromium-Nickel,Heat Resistant, for General Application |
HK30 | ASTM | USA | Steel Castings, Iron-Chromium and Iron-Chromium-Nickel,Heat Resistant, for General Application |