USA ASTM HK30 Steel Castings, Iron-Chromium and Iron-Chromium-Nickel,Heat Resistant, for General Application and HK30 Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
Category | Type | Steel Grade | Standard | Country | Application |
---|---|---|---|---|---|
Steel Grades | Special Alloy | HK30 | ASTM | USA | Steel Castings, Iron-Chromium and Iron-Chromium-Nickel,Heat Resistant, for General Application |
CG6MMN |
|||||
CG8M |
|||||
CK3MCuN |
|||||
CK20 |
|||||
CH8 |
|||||
CH10 |
|||||
CH20 |
|||||
CN3MN |
|||||
CN7M |
|||||
CT15C |
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
266 (≥) | 914 (≥) | 23 | 42 | 13 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 142 |
Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
---|---|---|---|---|---|---|---|
41 | - | - | 0.22 | - | |||
855 | 845 | - | 21.3 | 333 | - | ||
436 | - | 33 | 14.2 | 424 | 424 |
Heat treated : 1384°C - 1883°C
Grade | Standard | Country | Application |
---|---|---|---|
ASTM HK30 | AISI | USA | |
HK30 | ASTM | USA | Steel Castings, Iron-Chromium and Iron-Chromium-Nickel,Heat Resistant, for General Application |
HK30 | ASTM | USA | Steel Castings, Iron-Chromium and Iron-Chromium-Nickel,Heat Resistant, for General Application |
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...