Euronorm EN EN X80WMoCrV654 Euronorm Tool steel and EN X80WMoCrV654 Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
| Category | Type | Steel Grade | Standard | Country | Application |
|---|---|---|---|---|---|
| Steel Grades | Tool Steel And Hard Alloy | EN X80WMoCrV654 | EN | Euronorm | Euronorm Tool steel |
| EN 20N5CrMo2F |
|||||
| EN 20NiCrMo4F |
|||||
| EN 20NiCrMo7F |
|||||
| EN 20MoCrMo16 |
|||||
| EN 100Cr6 |
|||||
| EN l00CrMnS |
|||||
| EN 100CrMnMo7 |
|||||
| EN 100CrMo7 |
|||||
| EN X45Cr13 |
|||||
| EN X75WCrV1841 |
| C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Mo(%) | V(%) | W(%) |
|---|---|---|---|---|---|---|---|---|
| 0.70-0.88 | Max 0.40 | Max 0.40 | 0.030 | 0.030 | 3.80-4.50 | 4.70-5.20 | 1.70-2.00 | 6.00-6.70 |
| Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
|---|---|---|---|---|---|---|
| 124 (≥) | 467 (≥) | 41 | 14 | 32 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 231 |
| Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
|---|---|---|---|---|---|---|---|
| 24 | - | - | 0.13 | - | |||
| 974 | 136 | - | 13.3 | 322 | - | ||
| 266 | - | 23 | 14.2 | 242 | 414 |
Heat treated : 1462°C - 1364°C
| Grade | Standard | Country | Application |
|---|---|---|---|
| EN X80WMoCrV654 | EN | Euronorm | Euronorm Tool steel |
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...
Rfq.: sales@longhaisteel.com