C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Ni(%) | Mo(%) | V(%) |
---|---|---|---|---|---|---|---|---|
0.24-0.31 | 0.15-0.35 | 0.20-0.40 | Max 0.030 | Max 0.030 | 0.30-0.50 | 4.20-4.70 | 1.15-1.25 | 0.15-0.20 |
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
765 (≥) | 865 (≥) | 41 | 42 | 22 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 343 |
Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
---|---|---|---|---|---|---|---|
42 | - | - | 0.34 | - | |||
546 | 245 | - | 22.3 | 234 | - | ||
284 | - | 23 | 24.2 | 331 | 242 |
Heat treated : 1234°C - 1618°C