Romania STAS/SR R52 Structural steel and R52 Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
| Category | Type | Steel Grade | Standard | Country | Application | 
|---|---|---|---|---|---|
| Steel Grades | Structure Steel | R52 | STAS/SR | Romania | Structural steel | 
| A21 | |||||
| 26MnSil7 | |||||
| 9SiMn16 | |||||
| 10Ni35 | |||||
| HSiMn10 | |||||
| RV510 | |||||
| A4 | |||||
| A5 | |||||
| R37 | |||||
| R44 | 
| C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | V(%) | Cu(%) | Al(%) | 
|---|---|---|---|---|---|---|---|---|
| Min 0.18 | 0.17-0.45 | 1.05-1.65 | 0.035 | 0.035 | Min 0.30 | Min 0.15 | 0.30 | Min 0.025 | 
| Yield Rp0.2 (MPa) | Tensile Rm (MPa) | Impact KV/Ku (J) | Elongation A (%) | Reduction in cross section on fracture Z (%) | As-Heat-Treated Condition | Brinell hardness (HBW) | 
|---|---|---|---|---|---|---|
| 399 (≥) | 943 (≥) | 41 | 41 | 32 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 433 | 
| Temperature (°C) | Modulus of elasticity (GPa) | Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) | Specific thermal capacity (J/kg·°C) | Specific electrical resistivity (Ω mm²/m) | Density (kg/dm³) | Poisson’s coefficient, ν | 
|---|---|---|---|---|---|---|---|
| 41 | - | - | 0.42 | - | |||
| 544 | 943 | - | 32.3 | 111 | - | ||
| 389 | - | 32 | 43.2 | 132 | 124 | 
Heat treated : 1695°C - 1359°C
| Grade | Standard | Country | Application | 
|---|---|---|---|
| R52 | STAS/SR | Romania | Structural steel | 
| 100VMoCr52 | STAS/SR | Romania | tool steel | 
| 39VSiMoCr52 | STAS/SR | Romania | tool steel | 
| 40VSiMoCr52 | STAS/SR | Romania | tool steel | 
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...
Rfq.: sales@longhaisteel.com