Euronorm EN EN 35CrNiMo6KD Euronorm Structural steel and EN 35CrNiMo6KD Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
| Category | Type | Steel Grade | Standard | Country | Application |
|---|---|---|---|---|---|
| Steel Grades | Structure Steel | EN 35CrNiMo6KD | EN | Euronorm | Euronorm Structural steel |
| EN 15Cr2KD |
|||||
| EN 16MnCr5KD |
|||||
| EN 18CrMo4KD |
|||||
| EN 20MoCr4KD |
|||||
| EN 20NiCrMo2KD |
|||||
| EN 25CrMo4KD |
|||||
| EN 30CrNiMo8KD |
|||||
| EN 30NiCrMo2KD |
|||||
| EN 34Cr4KD |
|||||
| EN 34CrMo4KD |
| C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Ni(%) | Mo(%) |
|---|---|---|---|---|---|---|---|
| 0.32-0.39 | 0.is-0.40 | 0.50-0.80 | 0.035 | 0.035 | 1.30-1.70 | 1.30-1.70 | 0.15-0.30 |
| Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
|---|---|---|---|---|---|---|
| 978 (≥) | 628 (≥) | 12 | 41 | 14 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 312 |
| Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
|---|---|---|---|---|---|---|---|
| 24 | - | - | 0.41 | - | |||
| 779 | 962 | - | 24.3 | 311 | - | ||
| 357 | - | 34 | 12.2 | 333 | 312 |
Heat treated : 1319°C - 1894°C
| Grade | Standard | Country | Application |
|---|---|---|---|
| EN 35CrNiMo6KD | EN | Euronorm | Euronorm Structural steel |
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...