Euronorm EN EN 10MnSiMo835KE Euronorm Structural steel and EN 10MnSiMo835KE Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
Category | Type | Steel Grade | Standard | Country | Application |
---|---|---|---|---|---|
Steel Grades | Structure Steel | EN 10MnSiMo835KE | EN | Euronorm | Euronorm Structural steel |
EN C35BKD |
|||||
EN C35KD |
|||||
EN C45KD |
|||||
EN 1CE8 |
|||||
EN 2CEB |
|||||
EN 9MnMo25KE |
|||||
EN 9MnSi53KE |
|||||
EN 10MnSi63KE |
|||||
EN 10MnSi74KE |
|||||
EN ]0MnSiMo535KE |
C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Ni(%) | Mo(%) |
---|---|---|---|---|---|---|---|
<0.12 | 0.55 -0.75 | 1.75-2.05 | 0.025 | 0.025 | 0.15 | 0.15 | 0.40-0.60 |
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
296 (≥) | 713 (≥) | 31 | 11 | 34 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 213 |
Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
---|---|---|---|---|---|---|---|
14 | - | - | 0.32 | - | |||
752 | 872 | - | 43.3 | 311 | - | ||
155 | - | 41 | 44.2 | 111 | 313 |
Heat treated : 1232°C - 1513°C
Grade | Standard | Country | Application |
---|---|---|---|
EN 10MnSiMo835KE | EN | Euronorm | Euronorm Structural steel |