Spain UNE 20NiCrMoS2-2 Spain structural alloy steel and 20NiCrMoS2-2 Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
| Category | Type | Steel Grade | Standard | Country | Application |
|---|---|---|---|---|---|
| Steel Grades | Structure Steel | 20NiCrMoS2-2 | UNE | Spain | Spain structural alloy steel |
| 18CrMoS4 |
|||||
| 18CrNiMo7-6 |
|||||
| 18NiCr5-4 |
|||||
| 20MnCr5 |
|||||
| 20MnCrS5 |
|||||
| 20MoCr3 |
|||||
| 20MoCr4 |
|||||
| 20MoCrS3 |
|||||
| 20MoCrS4 |
|||||
| 20NiCrMo2-2 |
| Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
|---|---|---|---|---|---|---|
| 618 (≥) | 633 (≥) | 14 | 31 | 13 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 324 |
| Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
|---|---|---|---|---|---|---|---|
| 43 | - | - | 0.23 | - | |||
| 341 | 824 | - | 13.3 | 444 | - | ||
| 755 | - | 43 | 34.2 | 241 | 243 |
Heat treated : 1821°C - 1171°C
| Grade | Standard | Country | Application |
|---|---|---|---|
| 20NiCrMoS2-2 | UNE | Spain | Spain structural alloy steel |
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...