X4CrNiMoN25-7 Stainless Steel and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
| Category | Type | Steel Grade | Standard | Country | Application |
|---|---|---|---|---|---|
| Steel Grades | Stainless Steel | X4CrNiMoN25-7 | |||
| X1CrNiMoCu32-28-7 |
|||||
| X1NiCrMoCuN31-27-4 |
|||||
| X2CrNiMnMoNbN 25-18-5-4 |
|||||
| X3CrNiCu 18-9-4 |
|||||
| X7CrNiAl 17-7 |
|||||
| X6CrNiMo17-12-2 |
|||||
| X10CrNiMoTi 18-12 |
|||||
| X1CrNiMoNb 28-4-2 |
|||||
| X3CrNiMoTi 25-25 |
|||||
| X6CrNiMoNb17-12-2 |
| C |
Si ≤ |
Mn ≤ |
P ≤ |
S ≤ |
Cr | Ni | Mo | Other |
|---|---|---|---|---|---|---|---|---|
| ≤0.06 | 1.00 | 2.00 | 0.045 | 0.030 | 24.0-26.0 | 6.50-7.50 | 1.30-2.00 | Nb≥10*C |
| Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
|---|---|---|---|---|---|---|
| 932 (≥) | 218 (≥) | 34 | 21 | 44 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 132 |
| Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
|---|---|---|---|---|---|---|---|
| 31 | - | - | 0.31 | - | |||
| 439 | 626 | - | 43.3 | 213 | - | ||
| 991 | - | 31 | 13.2 | 422 | 413 |
Heat treated : 1447°C - 1538°C
| Grade | Standard | Country | Application |
|---|---|---|---|
| X4CrNiMoN25-7 | DIN | Germany | Stainless steel |