X1NiCrMoCuN31-27-4 Stainless Steel and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
Category | Type | Steel Grade | Standard | Country | Application |
---|---|---|---|---|---|
Steel Grades | Stainless Steel | X1NiCrMoCuN31-27-4 | |||
X2CrNiTi18-2 |
|||||
X1CrNiMoCuN25-20-7 |
|||||
X1CrNiMoAl15-7-2 |
|||||
X90CrCoMoV17 |
|||||
X1CrNiMoCu25-20-5 |
|||||
X6CrNiTi18-10 |
|||||
X5NiCrCuNb16-4 |
|||||
X6CrNiNb18-10 |
|||||
X2CrNiAlTi32-20 |
|||||
X1CrNiMoCu32-28-7 |
C |
Si ≤ |
Mn ≤ |
P ≤ |
S ≤ |
Cr | Ni | Mo | Other |
---|---|---|---|---|---|---|---|---|
≤0.020 | 0.70 | 2.00 | 0.030 | 0.010 | 26.0-28.0 | 30.0-32.0 | 3.00-4.00 |
Cu 0.70-1.50 N 0.04-0.15 |
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
936 (≥) | 723 (≥) | 13 | 12 | 23 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 331 |
Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
---|---|---|---|---|---|---|---|
32 | - | - | 0.41 | - | |||
976 | 346 | - | 31.3 | 412 | - | ||
379 | - | 24 | 12.2 | 241 | 423 |
Heat treated : 1356°C - 1969°C
Grade | Standard | Country | Application |
---|---|---|---|
X1NiCrMoCuN31-27-4 | DIN | Germany | Stainless steel |