Germany DIN X90CrCoMoV17 Stainless steel and X90CrCoMoV17 Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
Category | Type | Steel Grade | Standard | Country | Application |
---|---|---|---|---|---|
Steel Grades | Special Steel | X90CrCoMoV17 | DIN | Germany | Stainless steel |
W-Nr 1.4511 |
|||||
X2CrTi12/X6CrTi12 |
|||||
W-Nr 1.4512 |
|||||
W-Nr 1.4521 |
|||||
X2CrMoTi18-2 |
|||||
W-Nr 1.4529 |
|||||
X1NiCrMoCuN25-20-7 |
|||||
X1CrNiMoAI15-7-2 |
|||||
W-Nr 1.4532 |
|||||
W-Nr 1.4535 |
C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Mo(%) | V(%) | Co(%) |
---|---|---|---|---|---|---|---|---|
0.85-0.95 | Max 1.00 | Max 1.00 | Max 0.045 | Max 0.030 | 15.5-17.5 | 0.40-0.60 | 0.20-0.30 | 1.20-1.80 |
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
874 (≥) | 237 (≥) | 41 | 33 | 14 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 211 |
Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
---|---|---|---|---|---|---|---|
33 | - | - | 0.44 | - | |||
156 | 961 | - | 14.3 | 432 | - | ||
186 | - | 41 | 22.2 | 244 | 332 |
Heat treated : 1429°C - 1148°C
Grade | Standard | Country | Application |
---|---|---|---|
X90CrCoMoV17 | DIN | Germany | Stainless steel |
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...
Rfq.: sales@longhaisteel.com