Category | Type | Steel Grade | Standard | Country | Application |
---|---|---|---|---|---|
Steel Grades | Special Steel | S12MolCr17 | STAS/SR | Romania | tool steel |
S10Mn1.5 |
|||||
S10Mo |
|||||
S10VCr1 |
|||||
S12Mn2Si |
|||||
S12Cr26Ni20 |
|||||
S12Mn2 |
|||||
S12MnlSiNilTi |
|||||
S12Mn1.5Mo |
|||||
S12Mn2Mo |
|||||
S12MoCr1 |
C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Ni(%) | Mo(%) |
---|---|---|---|---|---|---|---|
0.12 | Max 0.80 | Max 0.90 | 0.030 | 0.02 | 15.0-18.0 | Max 0.60 | 0.90-1.10 |
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
233 (≥) | 285 (≥) | 43 | 23 | 14 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 334 |
Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
---|---|---|---|---|---|---|---|
12 | - | - | 0.21 | - | |||
417 | 782 | - | 11.3 | 343 | - | ||
336 | - | 23 | 33.2 | 144 | 223 |
Heat treated : 1255°C - 1573°C
Grade | Standard | Country | Application |
---|---|---|---|
S12MolCr17 | STAS/SR | Romania | tool steel |
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...