Finland SFS G-X 6 CrNi 13 4 SFS 386 Cast steel 386. GX-6 CrNi 13 4 and G-X 6 CrNi 13 4 Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
| Category | Type | Steel Grade | Standard | Country | Application | 
|---|---|---|---|---|---|
| Steel Grades | Special Steel | G-X 6 CrNi 13 4 | SFS | Finland | SFS 386 Cast steel 386. GX-6 CrNi 13 4 | 
| EN X12CrNiMoV12-3 | |||||
| EN X12M5 | |||||
| EN X15CrMo5-1 | |||||
| EN X18CrMoNbVNi1-1 | |||||
| EN X22CrMoV12-1 | |||||
| 501 | |||||
| MARAGING (C) 300 | |||||
| 18Ni Maraging Steel | |||||
| Maraging 350 | |||||
| G-X 12 Cr 13 | 
| Yield Rp0.2 (MPa) | Tensile Rm (MPa) | Impact KV/Ku (J) | Elongation A (%) | Reduction in cross section on fracture Z (%) | As-Heat-Treated Condition | Brinell hardness (HBW) | 
|---|---|---|---|---|---|---|
| 154 (≥) | 364 (≥) | 12 | 11 | 32 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 131 | 
| Temperature (°C) | Modulus of elasticity (GPa) | Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) | Specific thermal capacity (J/kg·°C) | Specific electrical resistivity (Ω mm²/m) | Density (kg/dm³) | Poisson’s coefficient, ν | 
|---|---|---|---|---|---|---|---|
| 21 | - | - | 0.24 | - | |||
| 482 | 559 | - | 31.3 | 333 | - | ||
| 831 | - | 44 | 23.2 | 244 | 221 | 
Heat treated : 1179°C - 1639°C
| Grade | Standard | Country | Application | 
|---|---|---|---|
| G-X 6 CrNi 13 4 | SFS | Finland | SFS 386 Cast steel 386. GX-6 CrNi 13 4 | 