C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Ni(%) | Mo(%) | Cu(%) |
---|---|---|---|---|---|---|---|---|
3.07-0.11 | 0.55 | 1.10-1.90 | 0.025 | 0.015 | 23.3-24.7 | 12.2-13.8 | Max 0.47 | 0.47 |
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
918 (≥) | 684 (≥) | 23 | 21 | 43 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 321 |
Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
---|---|---|---|---|---|---|---|
32 | - | - | 0.41 | - | |||
656 | 339 | - | 42.3 | 323 | - | ||
573 | - | 44 | 12.2 | 424 | 334 |
Heat treated : 1993°C - 1219°C
Grade | Standard | Country | Application |
---|---|---|---|
EN X9CrNi2413KE | EN | Euronorm | Euronorm Stainless Steel |
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...
Rfq.: sales@longhaisteel.com