Euronorm EN EN X90CrMoV18 Euronorm Stainless Steel and EN X90CrMoV18 Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
| Category | Type | Steel Grade | Standard | Country | Application | 
|---|---|---|---|---|---|
| Steel Grades | Special Steel | EN X90CrMoV18 | EN | Euronorm | Euronorm Stainless Steel | 
| EN X14CrMoS17 | |||||
| EN X17CrNi16-2 | |||||
| EN X20Cr13 | |||||
| EN X29CrS13 | |||||
| EN X30Cr13 | |||||
| EN X39Cr13 | |||||
| EN X39CrMo17-1 | |||||
| EN X46Cr13 | |||||
| EN X50CrMoV15 | |||||
| EN X70CrMo15 | 
| C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Mo(%) | V(%) | 
|---|---|---|---|---|---|---|---|
| 0.85-0.95 | 1.00 | 1.00 | 0.040 | 0.015 | 17.0-19.0 | 0.90-1.30 | 0.07-0.12 | 
| Yield Rp0.2 (MPa) | Tensile Rm (MPa) | Impact KV/Ku (J) | Elongation A (%) | Reduction in cross section on fracture Z (%) | As-Heat-Treated Condition | Brinell hardness (HBW) | 
|---|---|---|---|---|---|---|
| 764 (≥) | 983 (≥) | 13 | 31 | 31 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 134 | 
| Temperature (°C) | Modulus of elasticity (GPa) | Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) | Specific thermal capacity (J/kg·°C) | Specific electrical resistivity (Ω mm²/m) | Density (kg/dm³) | Poisson’s coefficient, ν | 
|---|---|---|---|---|---|---|---|
| 11 | - | - | 0.23 | - | |||
| 344 | 732 | - | 42.3 | 313 | - | ||
| 251 | - | 41 | 31.2 | 413 | 114 | 
Heat treated : 1635°C - 1132°C
| Grade | Standard | Country | Application | 
|---|---|---|---|
| EN X90CrMoV18 | EN | Euronorm | Euronorm Stainless Steel | 