C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Ni(%) | Mo(%) | Cu(%) | Nb(%) |
---|---|---|---|---|---|---|---|---|---|
0.070 | 0.70 | 1.00 | 0.040 | 0.015 | 13.0-15.0 | 5.00-6.00 | 1.20-2.00 | 1.20-2.00 | 0.15-0.60 |
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
627 (≥) | 959 (≥) | 12 | 43 | 41 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 122 |
Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
---|---|---|---|---|---|---|---|
23 | - | - | 0.24 | - | |||
955 | 214 | - | 34.3 | 233 | - | ||
695 | - | 33 | 31.2 | 221 | 323 |
Heat treated : 1674°C - 1778°C
Grade | Standard | Country | Application |
---|---|---|---|
EN X5CtNiMoCuNb14-5 | EN | Euronorm | Euronorm Stainless Steel |
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...
Rfq.: sales@longhaisteel.com