Euronorm EN EN X20CrMoWV12-1 Euronorm Stainless Steel and EN X20CrMoWV12-1 Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
Category | Type | Steel Grade | Standard | Country | Application |
---|---|---|---|---|---|
Steel Grades | Special Steel | EN X20CrMoWV12-1 | EN | Euronorm | Euronorm Stainless Steel |
EN X6NiCrTiMoVB25-15-2 |
|||||
EN X8CrCoNiMo10-6 |
|||||
EN X8CrNiNb16-13 |
|||||
EN X8NiCrAlTi32-21 |
|||||
EN X10CrMoV9-1 |
|||||
EN X12CrCoNi21-20 |
|||||
EN X12CrNiMoV12-3 |
|||||
EN X12CrNiWTiB16-13 |
|||||
EN X19CrMoNiNbVN11-1 |
|||||
EN X20CrMoV12-1 |
C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Ni(%) | Mo(%) |
---|---|---|---|---|---|---|---|
0.17-0.24 | 0.10-0.50 | 0.30-0.80 | 0.025 | 0.015 | 11.0-12.5 | 0.30-0.80 | 0.80-1.20 |
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
881 (≥) | 115 (≥) | 31 | 13 | 22 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 232 |
Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
---|---|---|---|---|---|---|---|
41 | - | - | 0.32 | - | |||
349 | 267 | - | 34.3 | 212 | - | ||
542 | - | 41 | 42.2 | 424 | 144 |
Heat treated : 1977°C - 1147°C
Grade | Standard | Country | Application |
---|---|---|---|
X20CrMoWV12-1 | DIN | Germany | The high-temperature and high-strength steel |
EN X20CrMoWV12-1 | EN | Euronorm | Euronorm Stainless Steel |
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...