Euronorm EN EN NiCr23Co12Mo Euronorm Stainless Steel and EN NiCr23Co12Mo Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
Category | Type | Steel Grade | Standard | Country | Application |
---|---|---|---|---|---|
Steel Grades | Special Steel | EN NiCr23Co12Mo | EN | Euronorm | Euronorm Stainless Steel |
EN X5BCrMnNiN20-8 |
|||||
EN X85CrMoV18-2 |
|||||
EN CoCr20W15Ni |
|||||
EN NiCo20Cr20MoTi |
|||||
EN NiCr15Fe7Ti2Al |
|||||
EN NiCr19Fe19Nb5Mo3 |
|||||
EN NiCr20Co13Mo4Ti3Al |
|||||
EN NiCr20Co18Ti |
|||||
EN NiCr20TiAl |
|||||
EN NiCr22Fe18Mo |
C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Mo(%) | Ti(%) |
---|---|---|---|---|---|---|---|
0.05-0.10 | 0.20 | 0.20 | 0.010 | 0.010 | 20.0-23.0 | 8.50-10.0 | 0.20-0.60 |
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
275 (≥) | 382 (≥) | 43 | 31 | 24 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 421 |
Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
---|---|---|---|---|---|---|---|
42 | - | - | 0.44 | - | |||
597 | 445 | - | 24.3 | 133 | - | ||
789 | - | 44 | 32.2 | 421 | 213 |
Heat treated : 1215°C - 1498°C
Grade | Standard | Country | Application |
---|---|---|---|
EN NiCr23Co12Mo | EN | Euronorm | Euronorm Stainless Steel |
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...
Rfq.: sales@longhaisteel.com