Euronorm EN EN NiCr15Fe8 Euronorm Stainless Steel and EN NiCr15Fe8 Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
| Category | Type | Steel Grade | Standard | Country | Application |
|---|---|---|---|---|---|
| Steel Grades | Special Steel | EN NiCr15Fe8 | EN | Euronorm | Euronorm Stainless Steel |
| EN X3CrNiMoN27-5-2 |
|||||
| EN X4CrNiMo16-5-1 |
|||||
| EN X5CrNi18-10 |
|||||
| EN XSCrNiCuNb16-4 |
|||||
| EN X5CrNiMo17-12-2 |
|||||
| EN X6Cr17 |
|||||
| EN X6CrAl13 |
|||||
| EN XeCrNiMoTi17-12-2 |
|||||
| EN X6CrNiNb18-10 |
|||||
| EN X6CrNiTi18-10 |
| C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Ni(%) | Ti(%) |
|---|---|---|---|---|---|---|---|
| 0.05-0.10 | 0.50 | 1.00 | 0.020 | 0.015 | 14.0-17.0 | Min72.0 | Max 0.30 |
| Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
|---|---|---|---|---|---|---|
| 231 (≥) | 733 (≥) | 23 | 43 | 11 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 244 |
| Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
|---|---|---|---|---|---|---|---|
| 34 | - | - | 0.33 | - | |||
| 326 | 742 | - | 14.3 | 332 | - | ||
| 582 | - | 22 | 31.2 | 321 | 412 |
Heat treated : 1482°C - 1673°C
| Grade | Standard | Country | Application |
|---|---|---|---|
| ISO NiCr15Fe8 | ISO | ISO | ISO standard heat-resisting alloy |
| EN NiCr15Fe8 | EN | Euronorm | Euronorm Stainless Steel |