Euronorm EN EN 41NiCrMo7-3-2 Euronorm Stainless Steel and EN 41NiCrMo7-3-2 Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
Category | Type | Steel Grade | Standard | Country | Application |
---|---|---|---|---|---|
Steel Grades | Special Steel | EN 41NiCrMo7-3-2 | EN | Euronorm | Euronorm Stainless Steel |
EN GX12Cr12 |
|||||
EN 19MnB4 |
|||||
EN 20CrMoVTiB4-10 |
|||||
EN 20Mn5 |
|||||
EN 21CrMoV5-7 |
|||||
EN 25CrMo4 |
|||||
EN 30CrNiMoS |
|||||
EN 34CrNiMo6 |
|||||
EN 35B2 |
|||||
EN 40CrMoV4-6 |
C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Ni(%) | Mo(%) |
---|---|---|---|---|---|---|---|
0.38-0.44 | 0.30 | 0.¢0-0.90 | 0.025 | 0.025 | 0.70-0.90 | 1.65-2.-00 | 0.15-0.30 |
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
979 (≥) | 483 (≥) | 14 | 32 | 33 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 212 |
Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
---|---|---|---|---|---|---|---|
23 | - | - | 0.43 | - | |||
393 | 322 | - | 34.3 | 444 | - | ||
996 | - | 11 | 23.2 | 443 | 213 |
Heat treated : 1493°C - 1667°C
Grade | Standard | Country | Application |
---|---|---|---|
EN 41NiCrMo7-3-2 | EN | Euronorm | Euronorm Stainless Steel |
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...
Rfq.: sales@longhaisteel.com