China GBT ZG30Cr26Ni5 Heat resistant cast steel and ZG30Cr26Ni5 Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
Category | Type | Steel Grade | Standard | Country | Application |
---|---|---|---|---|---|
Steel Grades | Special Alloy | ZG30Cr26Ni5 | GBT | China | Heat resistant cast steel |
ZG35Ni24Cr18Si2 |
|||||
ZG30Ni35Cr15(ZG3Ni35Cr15) |
|||||
ZG45Ni35Cr26 |
|||||
ZG40Cr22Ni4N(ZG4Cr22Ni4N) |
|||||
ZG30Cr25Ni20(ZG3Cr25Ni20) |
|||||
ZG20Cr20Mn9Ni2SiN(ZG2Cr20Mn9Ni2SiN) |
|||||
ZG08Cr18Ni12Mo2Ti(ZG0Cr18Ni12Mo2Ti) |
|||||
ZG40Cr9Si2 |
|||||
ZG30Cr18Mn12Si2N |
|||||
ZG35Cr24Ni7SiN |
C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Ni(%) | Mo(%) |
---|---|---|---|---|---|---|---|
0.20-0.40 | ≤2.00 | ≤1.00 | 0.04 | 0.04 | 24.0-28.0 | 4.00-6.00 | ≤0.50 |
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
415 (≥) | 832 (≥) | 43 | 41 | 44 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 131 |
Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
---|---|---|---|---|---|---|---|
32 | - | - | 0.22 | - | |||
761 | 355 | - | 43.3 | 331 | - | ||
412 | - | 22 | 24.2 | 213 | 431 |
Heat treated : 1161°C - 1828°C
Grade | Standard | Country | Application |
---|---|---|---|
ZG30Cr26Ni5 | GBT | China | Heat resistant cast steel |
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...
Rfq.: sales@longhaisteel.com