Korea KS STS305 KS standard austenite stainless steel bars(KS D3706-1992) and STS305 Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
Category | Type | Steel Grade | Standard | Country | Application |
---|---|---|---|---|---|
Steel Grades | Special Alloy | STS305 | KS | Korea | KS standard austenite stainless steel bars(KS D3706-1992) |
STS301 |
|||||
STS302 |
|||||
STS303 |
|||||
STS303Se |
|||||
STS304 |
|||||
STS304L |
|||||
STS304N1 |
|||||
STS304N2 |
|||||
STS304LN |
|||||
STS304J3 |
C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Ni(%) |
---|---|---|---|---|---|---|
Max 0.12 | Max 1.00 | Max 2.00 | Max 0.045 | Max 0.03 | 17.0-19.0 | 10.5-13.0 |
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
128 (≥) | 499 (≥) | 24 | 12 | 44 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 324 |
Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
---|---|---|---|---|---|---|---|
22 | - | - | 0.42 | - | |||
638 | 812 | - | 32.3 | 343 | - | ||
951 | - | 42 | 14.2 | 241 | 141 |
Heat treated : 1319°C - 1469°C
Grade | Standard | Country | Application |
---|---|---|---|
STS305 | KS | Korea | KS standard austenite stainless steel bars(KS D3706-1992) |
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...