China GBT K211 Age hardening type iron base alloy and K211 Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
Category | Type | Steel Grade | Standard | Country | Application |
---|---|---|---|---|---|
Steel Grades | Special Alloy | K211 | GBT | China | Age hardening type iron base alloy |
GH4145 |
|||||
GH4146 |
|||||
GH4151 |
|||||
GH4180 |
|||||
GH4220 |
|||||
GH4302 |
|||||
GH4698 |
|||||
GH4710 |
|||||
GH4738 |
|||||
GH4761 |
C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Ni(%) | W(%) | B(%) | Fe(%) |
---|---|---|---|---|---|---|---|---|---|
0.10-0.20 | Max 0.4 | Max 0.5 | Max 0.04 | Max 0.04 | 1.95-20.5 | 45.0-47.0 | 7.50-8.50 | 0.03-0.05 | Balance |
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
298 (≥) | 161 (≥) | 24 | 12 | 12 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 142 |
Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
---|---|---|---|---|---|---|---|
12 | - | - | 0.11 | - | |||
711 | 973 | - | 14.3 | 334 | - | ||
912 | - | 23 | 41.2 | 121 | 432 |
Heat treated : 1981°C - 1531°C