China GBT K18B conventional cast superalloy and K18B Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
| Category | Type | Steel Grade | Standard | Country | Application |
|---|---|---|---|---|---|
| Steel Grades | Special Alloy | K18B | GBT | China | conventional cast superalloy |
| K418B |
|||||
| K419 |
|||||
| K419H |
|||||
| K8 |
|||||
| K9 |
|||||
| K12 |
|||||
| K17 |
|||||
| K17G |
|||||
| K17L |
|||||
| K18 |
| C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Ni(%) | Mo(%) | Cu(%) | Co(%) | B(%) | Nb(%) | Al(%) | Ti(%) | Fe(%) |
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| 0.03-0-07 | 0.50 | 0.25 | 0.015 | 0.015000000000000000 | 11.00-13.00 | Bal | 3.80-5.20 | 0.500 | ≤1.00 | 0.005-0.015 | 1.50-2.50 | 5.50-6.50 | 0.40-1.00 | ≤0.50 |
| Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
|---|---|---|---|---|---|---|
| 879 (≥) | 664 (≥) | 41 | 43 | 12 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 432 |
| Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
|---|---|---|---|---|---|---|---|
| 21 | - | - | 0.13 | - | |||
| 819 | 246 | - | 43.3 | 113 | - | ||
| 247 | - | 12 | 22.2 | 111 | 123 |
Heat treated : 1269°C - 1569°C
| Grade | Standard | Country | Application |
|---|---|---|---|
| K418B | GBT | China | conventional cast superalloy |
| K18B | GBT | China | conventional cast superalloy |
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...