USA UNS J93401 Steel Castings, Iron-Chromium and Iron-Chromium-Nickel,Heat Resistant, for General Application and J93401 Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
Category | Type | Steel Grade | Standard | Country | Application |
---|---|---|---|---|---|
Steel Grades | Special Alloy | J93401 | UNS | USA | Steel Castings, Iron-Chromium and Iron-Chromium-Nickel,Heat Resistant, for General Application |
J92971 |
|||||
J92972 |
|||||
J93970 |
|||||
J92802 |
|||||
J92999 |
|||||
J93790 |
|||||
J93000 |
|||||
J93254 |
|||||
J93202 |
|||||
J93400 |
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
316 (≥) | 437 (≥) | 42 | 33 | 32 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 334 |
Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
---|---|---|---|---|---|---|---|
24 | - | - | 0.14 | - | |||
863 | 288 | - | 21.3 | 411 | - | ||
874 | - | 23 | 41.2 | 112 | 233 |
Heat treated : 1677°C - 1933°C
Grade | Standard | Country | Application |
---|---|---|---|
UNS J93401 | AISI | USA | |
J93401 | UNS | USA | Steel Castings, Iron-Chromium and Iron-Chromium-Nickel,Heat Resistant, for General Application |
J93401 | UNS | USA | Steel Castings, Iron-Chromium and Iron-Chromium-Nickel,Heat Resistant, for General Application |
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...
Rfq.: sales@longhaisteel.com